Visit
Official Website

Plasmost Enterprise Sdn Bhd
47, Lorong Perusahaan Ringan Juru 1,
Kawasan Perusahaan Ringan Juru, Juru,
14100 Bukit Mertajam,
Penang, Malaysia.
+604-5074613
+604-5074713
+604-5024613
0194804613
Kuala Lumpur Office
E-2-22, IOI Boulevard, Jalan Kenari 5, Bandar Puchong Jaya, 47170 Selangor, Malaysia.
+603-80737346
+603-80737346

Singapore Office
65, Sims Avenue, #04-03, Yi Xiu Factory Building, Singapore, 387418.
+65-90092991
+65-68462505

Cross Cutter

Previous 6 / 6 Next

Quantity
Add Quotation


Download Files

Cross-Cut_Tester.pdf (581.23 KB)

In order to perform satisfactorily, coatings must adhere to the substrates on which they are applied. In practice, three different test procedures are used to assess the resistance of paints and coatings to separation from substrates.

Cross-Cut Test
This test method specifies a procedure for assessing the resistance of paints and coatings to separation from substrates when a rightangle lattice pattern is cut into the coating, penetrating through to the substrate.

The method may be used for a quick pass/fail test. When applied to a multi-coat system, assessment of the resistance to separation of individual layers of the coating from each other may be made.

Scrape Adhesion
This test method covers the determination of the adhesion of organic coatings such as paint, varnish, and lacquer when applied to smooth, flat (planar) panel surfaces. It has been found useful in providing relative ratings for a series of coated panels exhibiting significant differences in adhesion.

The materials under test are applied at uniform thickness to flat panels, usually sheet metal of uniform surface texture. After drying, the adhesion is determined by pushing the panels beneath a rounded stylus or loop that is loaded with increasing amounts of weight until the coating is removed from the substrate surface.

Pull-Off Test
Adhesion of a single coating or a multi-coat system of paint, varnish or related products is assessed by measuring the minimum tensile stress necessary to detach or rupture the coating in a direction perpendicular to the substrate. This method maximizes tensile stress as compared to the shear stress applied by other methods such as scratch adhesion and results may not be comparable.

The test is performed by securing a loading fixture (dolly) perpendicular to the surface of the coating with an adhesive. After the adhesive is cured, a testing apparatus is attached to the loading fixture and aligned to apply tension perpendicular to the test surface. The force applied is gradually increased and monitored until either a plug of coating material is detached, or a specified value is reached.

Please leave your enquiry here, we will reply as soon as possible.
Name*  
Company Name  
Product Interested  
Quantity  
Email*  
Contact No.*  
Messages*  
   

You have 0 items in you cart. Would you like to checkout now?
0 items
Subscribe Newsletter